Research Progress in Thermal Expansion Characteristics of TATB-based Polymer Bonded Explosives

Published 15 December, 2023

Under complex temperature variations, the irreversible thermal expansion of polymer-bonded explosives (PBXs) containing 1,3,5-triamino-2,4,6-trinitrobenzene (TATB) leads to diminished shape stability. This, in turn, directly impacts the mechanical properties and safety performance during storage and use. In recent years, extensive and thorough research has been carried out to investigate the thermal expansion characteristics of TATB-based explosives.

In a study published in the KeAi journal Energetic Materials Frontiers, a group of researchers from China, explored the distinctive crystal structure of TAT and the thermal expansion mechanism of TATB-based PBXs. Additionally, they summarized the microstructural evolution during the thermal expansion process and analyzed the consequential effects of thermal expansion on the overall performance of these explosives.

“More attention was paid to the influencing factors of thermal expansion and control methods. Evidently, designing a new structure of negative thermal expansion binding system, through the design of negative thermal expansion polymers or fillers and positive expansion TATB crystals, can reduce the linear expansion coefficient of PBXs,” explained the study’s lead author Cong-mei Lin. “This approach not only suppresses material thermal expansion but also holds broad application prospects.”

Notably, suppressing the irreversible thermal expansion of TATB-based PBXs and improving the shape stability of the explosive under a temperature cycling environment is important. However, effectively suppressing the thermal expansion of TATB-based PBXs remains a challenge.

"Going forward, we need to focus on the irreversible expansion mechanism of TATB-based PBXs; TATB crystal structure design and control; the design and development of new structural-functional integrated polymers; and the application of new negative thermal expansion functional materials."

The authors believe that the development of the structural design of TATB and binder system and the application of negative thermal expansion functional materials will bring new opportunities to suppress the thermal expansion of TATB-based PBXs and enrich the modification techniques of energetic composites.

Image: IRREVERSIBLE THERMAL EXPANSION IN TATB BASED PBXS. CREDIT: THE AUTHORS

Contact author details: Yu-shi Wen, Institute of Chemical Materials, CAEP, Mianyang, China, wenys@caep.cn

Funder: This research was supported by the National Natural Science Foundation of China (Grant No. U213020030).

Conflict of interest: The authors declare that they have no known competing financial interests or personal relationships that could have appeared to influence the work reported in this paper.

See the article: Cong-mei Lin, Liang-fei Bai, Zhi-jian Yang, Fei-yan Gong, Yu-shi Wen, Research progress in thermal expansion characteristics of TATB based polymer bonded explosives, Energetic Materials Frontiers, Volume 4, Issue 3, 2023. https://doi.org/10.1016/j.enmf.2023.09.003